Dissertation > Excellent graduate degree dissertation topics show
Quickly-Formed Self-lubricating Hard Coating on Surface of Aluminum Alloy
Author: LuChuang
Tutor: ZhouZuoï¼›XiongRenZhang
School: Nanjing University of Technology and Engineering
Course: Materials Science and Engineering
Keywords: Aluminum alloy Self - lubricating coatings Friction properties Corrosion resistance Hardness
CLC: TG174.4
Type: Master's thesis
Year: 2009
Downloads: 86
Quote: 0
Read: Download Dissertation
Abstract
|
In this paper, a fast self-lubricating hard coating method for preparing the surface of an aluminum alloy , the method is for lubrication modifier the MoS 2 < / sub > particles using symbiotic deposition method on the aluminum hard anodizing process will MoS the 2 < / sub > particle deposition of in hard anodized film of the aluminum alloy , in order to achieve the purpose of improving the lubricating properties of film . By orthogonal experiment method to study the sulfuric acid - sulfuric acid - based oxalic acid mixed acid electrolyte system components and process parameters on the law of self-lubricating coating growth process and performance by scanning electron microscopy ( SEM ) , can spectroscopy (EDS) and other methods to observe the structural characteristics of the aluminum alloy self-lubricating coating , measured MoS 2 in the film distribution ; through the salt spray test , non-destructive thickness , which was means of micro hardness tester, micro friction tester equipment film corrosion , hardness, wear-resistant properties . Spectroscopy (EDS) analysis results show that the uniform distribution of the film prepared by the symbiotic deposition method four elements such as Al , O , Mo , S , Mo , S , of the total mass of 10 % ; friction performance test results produced by this method the film coefficient of friction of 0.2 , far lower than the friction coefficient of the hard oxide layer of 0.9 , and further confirmed that the film not only exist the MoS 2 < / sub > , and the MoS 2 < / sub > to improve the the lubricating performance of the film ; thickness test results show that the use of double-pulse current mode , in the joint under the effect of the additive aluminum hard self-lubricating film growth rate significantly increased , maximum growth rate 4um/min , is a conventional hard anodizing . 2 times; the test results of the salt spray test results of scanning electron microscopy (SEM) analysis of symbiotic aperture film deposition method becomes small, low porosity ; hardness test results show that the microhardness of the surface of the film prepared by this method is slightly improved ; the corrosion resistance is proportional to the film thickness of the film .
|
Related Dissertations
- Numerical Simulation and Experiment on Hydroforming of Cups with Controllable Radial Pressure,TG386
- Synthesis and Application of the chloro- methoxy fatty acid methyl esters,TQ414.8
- Prototype Development of Intimate Apparel Mannequin,TS941.2
- Molecular Identification of Hardness-related Genes and Analysis of Molecular Mechanism of PINA Null in Bread Wheat,S512.1
- Electroless Ni-Pon the Bulk Nanocrystalline Ingot Iron,TQ153.1
- Construction of RNA Interference Vectors of Pin Genes Determining Grain Hardness and Genetic Transformation in Wheat,S512.1
- Preparation, Characterization and Performance of the Bio-coatings on the Surface of Pure Titanium Based on Micro Arc Oxidation,R318.08
- Magnetron sputtering B-C-N film and Characterization,O484.1
- Vacuum casting AZ91 Magnesium Alloy Corrosion Resistance,TG146.22
- Stitching hardened steel ball head milling force modeling and simulation and experimental study,TG54
- Submarine hydrothermal organisms Sampler key technology research,TH766
- The Study on Red Soil Corrosion by the Technological Direct, Continuous Monitoring,X53
- Evolution of Shear Band, Free Volume and Hardness of as Rolled Zr-based Bulk Metallic Glasses,TG339
- Effect of the Rubbing and Wearing Behavior of Steel Rail by Ultrasonic Peening,TG115.58
- Fabrication and Tribological Properties of DLC Films Deposited by MF-PCVD,TG174.4
- Effects of Electrical Parameters on Microstructure and Corrosion Resistance of Micro-arc Oxidation Coating on AZ91D Magnesium Alloys under Different Power Supply,TG174.4
- Semi-solid Billets Preparation and Its Deforming Numerical Simulation of 6xxx Aluminum Alloy,TG249.9
- Copper surface metal clips embedded ceramic composite coating technology research,TG174.44
- Research on Squeeze Casting Technology for High Strength and Toughness Aluminum Alloy Parts,TG249.2
- Hot Deformation Behavior of 2026 Aluminum Alloy at Elevated Temperature,TG146.21
- Of multistage solid solution heat treatment on the microstructure and properties of 7150 aluminum alloy,TG156.94
CLC: > Industrial Technology > Metallurgy and Metal Craft > Metallurgy and Heat Treatment > Metal corrosion protection,metal surface treatment > Corrosion control and protection > Metal surface protection technology
© 2012 www.DissertationTopic.Net Mobile
|